Day 13: Polymerization 1-Vinyl-3-(3-sulphopropyl)imidazolium hydroxide inner salt
[slideshow=10]
Day 13:
Success, managed to get the initator to work with the monomer at 60 degrees C without making the test tube explode during the nitrogen gas flussing step.
But with success there is slight failure where I could not open the top for the test tube glass device. Cooking it for another day to see if the cap will loosen. Probably use plyers if it doesnt work out tomorrow.